coral bowls
Moderators: Brad Walker, Tony Smith
coral bowls
I want to make a couple of small "coral" bowls. The tutorial I found used stainless bowls for shaping. Could I use my ball molds and slump or is there something about the spidery construction of these that wants to drape instead of slump? Of course these are for gifts that I need next week.
Vonon
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: coral bowls
Both are possible. Different effect
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/