Hi, we have a small fused glass business and want to keep expanding our tools for the studio. I was curious, of your thoughts on tools. We have a wet saw and grinder, and ringsaw, but are thinking about getting either a lapwheel sander or a sanding belt sander to do more of the coldworking/finishing. For those of you that do a lot of cold working on fused items (usually plates, small dishes, jewelry - would you suggest our next purchase should be the lapwheel or a belt sander. What do most folks doing fused glass tend to prefer? We have a large non-profit studio where we can go to do some of this coldworking, but wanting to get more at home so we don't have to drive in. Any suggestions are appreciated.
Thanks
Cherie
Belt Sander or Lap Wheel
Moderators: Brad Walker, Tony Smith
-
Cherie Knopf
- Posts: 14
- Joined: Tue Apr 23, 2013 8:37 pm
- Location: Morgan Hill, California
- Contact:
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Belt Sander or Lap Wheel
Sander first then lap wheel...the bigger the better
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Re: Belt Sander or Lap Wheel
I agree, wet belt sander first, lapwheel second. The belt sander can be made to do flat surfaces (although it's not ideal) and straight edges, but it's tough to get a lap wheel to cover contours the way a belt sander can.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Belt Sander or Lap Wheel
what jim, cynthia and jim said
but
get bigger machines than you think you need.
In a year or so you will curse the benchtop sander and the 12" grinder.
but
get bigger machines than you think you need.
In a year or so you will curse the benchtop sander and the 12" grinder.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Belt Sander or Lap Wheel
I made an assumption, and we all know that assumptions are the mother of all screw ups :>)
I assumed that she would get the biggest one that she could afford.
The other Jim
I assumed that she would get the biggest one that she could afford.
The other Jim
-
misteroldhouse
- Posts: 10
- Joined: Tue Dec 04, 2007 1:02 am
- Location: Dallas, Texas
- Contact:
Re: Belt Sander or Lap Wheel
I agree with all, First the WBS, than a diamond lap.
In my experience, diamonds cut faster & deeper; one often has to use the WBS with t's silicon carbide wet belts in order to remove those fine diamond-produced scratches!
Larry
In my experience, diamonds cut faster & deeper; one often has to use the WBS with t's silicon carbide wet belts in order to remove those fine diamond-produced scratches!
Larry