Slumping schedule for float glass

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Lemonkitten
Posts: 1
Joined: Thu Dec 19, 2013 2:27 pm

Slumping schedule for float glass

Post by Lemonkitten »

Hello everyone. I am a Lampworker who is slowly getting into the wonderful art of fusing. Today a good friend of mine gave me a load of float glass. I have managed to get a good (I hope...) fusing schedule. However I simply can't find a schedule for slumping this glass into a mould. Does anyone have a slumping schedule for float. Obviously I understand the complexities of this glass and that each sheet could differ.....but a good basic start is all I require in centigrade please.
Thanks
Janey
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Slumping schedule for float glass

Post by Marty »

First- there's a temp conversion on this page.
Second- What kind of mold?
Tammy Macdonald
Posts: 15
Joined: Tue Jun 18, 2013 1:45 pm
Location: Texas

Re: Slumping schedule for float glass

Post by Tammy Macdonald »

http://glasswithapast.com/ has lots of information about float and/or recycled glass. It's worth checking out.

Good luck.