Cerium Oxide.. Alternative anyone?
Moderators: Brad Walker, Tony Smith
Cerium Oxide.. Alternative anyone?
At present I cold work using a bevel star lap wheel to trim my pendants finishing with Cerium Oxide polish rather than Fire polishing.. I really like the 'finish' and crispness this gives..
Cerium oxide has soared in Price, any suggestions as to an alternative that I could use on my Bevel Star Lap wheel?
Thanks..
Cerium oxide has soared in Price, any suggestions as to an alternative that I could use on my Bevel Star Lap wheel?
Thanks..
Re: Cerium Oxide.. Alternative anyone?
it's probably soared because most of it comes from chinese sources, and they have stopped exporting so much raw materials as in the past.
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Cerium Oxide.. Alternative anyone?
You could use pumice prior to your cerium and you will find that you need to use much less cerium. Must have a dedicated pumice pad though; cannot use the same one for the cerium.
Tim Yardic
Yardic Glassworks
Yardic Glassworks
Re: Cerium Oxide.. Alternative anyone?
I get a pretty good shine with cork. I agree with Tim; if you can prefinish well, you need much less cerium (or cork).
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Cerium Oxide.. Alternative anyone?
Where do you get pumice in USA?
Does hisglass carry this?
I mean for a foreigner like me..
THANKS,
HAVI
Does hisglass carry this?
I mean for a foreigner like me..
THANKS,
HAVI
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Warren Weiss
- Posts: 137
- Joined: Thu Mar 13, 2003 8:06 pm
- Location: Richmond, VA
Re: Cerium Oxide.. Alternative anyone?
Hi Havi,
I'm sure you can get pumice in Israel. It is a very common abraisive. Also used in hand soaps to get grime off.
Warren
I'm sure you can get pumice in Israel. It is a very common abraisive. Also used in hand soaps to get grime off.
Warren
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Cerium Oxide.. Alternative anyone?
I picked up my last batch of pumice from Covington Engineering.
www.covington-engineering.com
www.covington-engineering.com
Tim Yardic
Yardic Glassworks
Yardic Glassworks
Re: Cerium Oxide.. Alternative anyone?
Thanks Warren,Warren Weiss wrote:Hi Havi,
I'm sure you can get pumice in Israel. It is a very common abraisive. Also used in hand soaps to get grime off.
Warren
Do not be so sure.... I only managed to find places that sell blocks of pumice, not powder.
I assume it might be easier for me to buy it from Covington in USA....
Thanks anyway,
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Cerium Oxide.. Alternative anyone?
Pumice comes in various grades.. You can get a very fine 'flour pumice.. less abrasive than the regular.. Funny I didn't even think about Pumice, I have a box of the stuff!