Slumping- number of molds at once?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Amy Jakowski
Posts: 11
Joined: Sat Feb 16, 2013 1:21 pm

Slumping- number of molds at once?

Post by Amy Jakowski »

Thank you all for your input on buying a kiln. Now one more question before I take the plunge. Can I slump more than one mold in a Skutt Clamshell (20" shelf) or Skutt 1014 (22" shelf)? Will have side elements blocked from one mold cause a significant problem? Will location in a element top only kiln also cause a problem for multiple molds? Should just get a bigger kiln?
Thank you.
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Slumping- number of molds at once?

Post by charlie »

the # of molds you can slump in one load depends upon the size of the molds (floor space) and heat schedules each mold needs. some molds need very little and some need a lot of heatwork. if you use both in the same load, will one be overfired and the other underfired?
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Slumping- number of molds at once?

Post by Judd »

I have always places as many molds in my kiln as possible. As long as you are an inch or so away from the walls/elements, you should be fine. If your molds are unusually thick or heavy, I would fire up slowly, like 150 degrees per hour.
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Slumping- number of molds at once?

Post by Valerie Adams »

I saw this photo the other day and made a note of it to remind me that I could slump student work this way. I believe this was taken from a Patty Gray class.
molds.jpg
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Slumping- number of molds at once?

Post by JestersBaubles »

Valerie Adams wrote:I saw this photo the other day and made a note of it to remind me that I could slump student work this way. I believe this was taken from a Patty Gray class.
molds.jpg
Yep, that's a Patty Gray class :)

Dana W.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Slumping- number of molds at once?

Post by Brad Walker »

Valerie Adams wrote:I saw this photo the other day and made a note of it to remind me that I could slump student work this way.
The reason this works is that the molds are very gentle, with only a short drop. They're also molds that can stand being overfired or held at a long time at slumping temperature. And they're all the same mold.

If your molds are deeper or steeper, this kind of kiln loading will probably be problematical.
Alexis Dinno
Posts: 57
Joined: Sun Dec 13, 2009 9:35 pm

Re: Slumping- number of molds at once?

Post by Alexis Dinno »

In my experience low temperature slumps (~605º C) are problematic when 'shading' lower pieces from the top elements (when only top elements are on). Same goes for placing slumping molds on stacks of shelves.
Post Reply