How the heck do I read the measurements on a circle cutter?
Moderator: Tony Smith
-
Shelley Lewis
- Posts: 73
- Joined: Wed Dec 11, 2013 11:14 am
How the heck do I read the measurements on a circle cutter?
I've received my first circle cutter but it came with NO directions. I feel comfortable knowing how to actually cut the circle, but not how to set up the diameter for the cutting blade. The measurements on the arm are in mm, but the first marking is 6. It is then marked 7,8,9,10 and then repeats 1-9 and then 20. The first circle I want to cut is 5.25 inches diameter. Can someone please explain where to set the cutting blade? Seems like such an easy thing, but I find it confusing! ](./images/smilies/eusa_wall.gif)
-
Shelley Lewis
- Posts: 73
- Joined: Wed Dec 11, 2013 11:14 am
Re: How the heck do I read the measurements on a circle cutt
Ok, I finally figured it out! I'll leave this post up just in case another newbie needs help, so please feel free to reply!
Re: How the heck do I read the measurements on a circle cutt
I don't bother with those markings, I turn the thing over and use a ruler from the center of the pivot to the wheel.
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: How the heck do I read the measurements on a circle cutt
It depends upon the cutter. I have a crummy cheapo something or another that I can't figure out how to set up for the life of me (it also moves when you cut circles). And I have a lovely Silberschnitt that is easy to read/set up, stays put, and I get perfect circles every time. With this cutter, which is marked in both mm & inches, you move the cutting head to the mark for the number you want on the "inside" edge. That probably doesn't make sense
.
o---------------------| |------------
Center ^ Inside edge of head -- line that edge up with the value you want.
point
Every time I use the Silberschnitt cutter, I kiss a German
(my husband )
Dana W.
o---------------------| |------------
Center ^ Inside edge of head -- line that edge up with the value you want.
point
Every time I use the Silberschnitt cutter, I kiss a German
Dana W.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: How the heck do I read the measurements on a circle cutt
5.25" is 133.35mm or 13.33cmShelley Lewis wrote:I've received my first circle cutter but it came with NO directions. I feel comfortable knowing how to actually cut the circle, but not how to set up the diameter for the cutting blade. The measurements on the arm are in mm, but the first marking is 6. It is then marked 7,8,9,10 and then repeats 1-9 and then 20. The first circle I want to cut is 5.25 inches diameter. Can someone please explain where to set the cutting blade? Seems like such an easy thing, but I find it confusing!
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: How the heck do I read the measurements on a circle cutt
I have found the simplest way to use these circle cutters is to draw a pencil line on a piece of paper. Place the CC in the center of the line and gently "score" the paper. Measure carefully between the score lines and adjust until perfect . . .
-
judith
- Posts: 49
- Joined: Tue Mar 11, 2003 8:57 am
- Location: Vitrum Studio - Maryland - DC area
- Contact:
Re: How the heck do I read the measurements on a circle cutt
What Brock said. Then you're certain it will cut the exact size you need.
judith
NEW Spring 2014 session of classes on line.......Nathan Sandberg, Richard Parrish, Martha Pfanschmidt and more!
http://www.vitrumstudio.com
http://www.judithconwayglass.com
NEW Spring 2014 session of classes on line.......Nathan Sandberg, Richard Parrish, Martha Pfanschmidt and more!
http://www.vitrumstudio.com
http://www.judithconwayglass.com
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: How the heck do I read the measurements on a circle cutt
yep like they said. r.
artist, owner of wanchese art studio, marine finisher
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: How the heck do I read the measurements on a circle cutt
An alternative with the silberschnitt is to. Mark a cross at the centre of your circle. Measure your radius and mark it at one point on the glass (measured from the centre of the cross). Place the four marks on the central pivot part of the cutter, use the suction cup to secure. Then extend the cutter head until the wheel is in line withe the radius mark. Secure the head to the bar and score. This way you do not need the marks on the bar, which will wear away anyway over time