Pattern Bar Piece help plz
question- when one uses a saw on a pattern bar, the surface is left milky from the saw. I have a lot of clear in this particular pattern bar and I did a fuse the other day which failed for another reason. (volume control) What I didn't count on was the clear areas still retain some of that milky look instead of being crystal clear. Should I sandblast the pieces before including them in work? Should I firepolish before?
			
			
									
						
							"When I was a boy I was told that anybody could become President; 
I'm beginning to believe it."
-- Clarence Seward Darrow (1857-1938)
			
						I'm beginning to believe it."
-- Clarence Seward Darrow (1857-1938)
- 
				Richard Blummer
- Posts: 13
- Joined: Wed Jul 14, 2010 9:15 am
- Location: Egg Harbor Township, NJ
- Contact:
Re: Pattern Bar Piece help plz
It may be that your slices were not clean enough.  When I'm slicing up pattern bars, I drop the slices into a bucket of water as I go along, so that the swarf from the slicing does not have a chance to dry on the pieces, and still I scrub them thoroughly when setting them up for fusing.
			
			
									
						
							אָשֵׁר חַיִּים
			
						Re: Pattern Bar Piece help plz
thank you
			
			
									
						
							"When I was a boy I was told that anybody could become President; 
I'm beginning to believe it."
-- Clarence Seward Darrow (1857-1938)
			
						I'm beginning to believe it."
-- Clarence Seward Darrow (1857-1938)
- 
				jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Pattern Bar Piece help plz
I find that it is always a good idea to sandblast any pieces I have taken a saw to
			
			
									
						
							"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
			
						- 
				twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Pattern Bar Piece help plz
Hi!!! I do alot of work with pattern bars and do not have a sand blaster and the way I have found good success is to clean every single piece with just water and a green scrubby to get all the sawed water off and then I dry on clean paper towels and keep covered after each is totally dry. I have never had any scum on my pieces , so clean is good.    
Leslie
			
			
									
						
							Leslie
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
			
						website: http://www.twinvision.fusedglassartists.com