Anyone tried the 96 Coe black fires copper?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Cheryl Maahs
Posts: 3
Joined: Mon Jan 13, 2014 12:30 am

Anyone tried the 96 Coe black fires copper?

Post by Cheryl Maahs »

I bought some because I really like the idea of a metallic copper finish ... Just haven't found the nerve to "play" with it.

Have you capped it with clear - or - without? Does it really finish a metallic copper? Have any pics?

Thanks
S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: Anyone tried the 96 Coe black fires copper?

Post by S.TImmerman »

Test, test, test!

Try it one a small piece both ways -
Marian
Posts: 71
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: Anyone tried the 96 Coe black fires copper?

Post by Marian »

What is this? New glass color from Spectrum or a surface decoration to fire?