Does anyone have any advice about what type of glue to use to bond glass to an mdf wooden backing for framing? The piece I need to bond is about 12 x 10 x1 inches, so quite small but is pretty heavy, it probably weighs a couple of pounds. Transparency is not an issue as it is opaque on the base layer. I am thinking of using a heavy duty silicon like 'Stiks Like Sh•t' but am concerned it may not hold.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: bonding
GE Silicone II.
Get a fresh tube, thoroughly clean both surfaces, apply, wait 24 hours to let it cure fully.
We have glass to wood pieces hung with silicone that were created over a decade ago and are still going strong.
Other premium brands of silicone will work well, too.
By the way, this is a good site for bonding questions: http://www.thistothat.com
Get a fresh tube, thoroughly clean both surfaces, apply, wait 24 hours to let it cure fully.
We have glass to wood pieces hung with silicone that were created over a decade ago and are still going strong.
Other premium brands of silicone will work well, too.