Tetka thicker than 3MM

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
susanmozingo
Posts: 7
Joined: Sun Jun 06, 2004 4:12 pm

Tetka thicker than 3MM

Post by susanmozingo »

I can score and break 3mm Tetka without a problem. I break using either the Morton button or running pliers. If the piece of Tetka is thicker than 3MM I can't break the score. Do I need to press harder when I am scoring? Thanks.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Tetka thicker than 3MM

Post by Marty »

Don't score any harder.
You will need slightly more breaking pressure for the 4mm and considerably more for the 6mm.
Get yourself these for the 6mm: http://shop.bullseyeglass.com/tools-sup ... liers.html
I'm not sure about other (cheaper) sources for those, you'll have to do some research.
susanmozingo
Posts: 7
Joined: Sun Jun 06, 2004 4:12 pm

Re: Tetka thicker than 3MM

Post by susanmozingo »

Thank you
Post Reply