I can score and break 3mm Tetka without a problem. I break using either the Morton button or running pliers. If the piece of Tetka is thicker than 3MM I can't break the score. Do I need to press harder when I am scoring? Thanks.
Re: Tetka thicker than 3MM
Don't score any harder.
You will need slightly more breaking pressure for the 4mm and considerably more for the 6mm.
Get yourself these for the 6mm: http://shop.bullseyeglass.com/tools-sup ... liers.html
I'm not sure about other (cheaper) sources for those, you'll have to do some research.
You will need slightly more breaking pressure for the 4mm and considerably more for the 6mm.
Get yourself these for the 6mm: http://shop.bullseyeglass.com/tools-sup ... liers.html
I'm not sure about other (cheaper) sources for those, you'll have to do some research.