felt pen for signing fused work
Moderators: Brad Walker, Tony Smith
felt pen for signing fused work
I am wondering if anyone has come across a felt pen that can be permanent after firing. I am looking for an easy way to sign my fused glass. Using a diamond instrument is just too labor intensive.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: felt pen for signing fused work
Silver Sharpie won't burn off.
Re: felt pen for signing fused work
You can buy an electric/battery operated engraver pen that's much easier to use--if you rub a little Sharpie marker over the marks, you'll get a very legible, fine line that stays.
The metallic Sharpies will stay after firing, as Brad said. Dykem markers will, too. The only thing I don't like about them is that they make rather thick lines for smaller objects like jewelry, and I've had them flake a bit if they were on the outside of the glass where the piece saw lots of wear (as in jewelry). With a little advanced planning, though, you can overcome that.
The metallic Sharpies will stay after firing, as Brad said. Dykem markers will, too. The only thing I don't like about them is that they make rather thick lines for smaller objects like jewelry, and I've had them flake a bit if they were on the outside of the glass where the piece saw lots of wear (as in jewelry). With a little advanced planning, though, you can overcome that.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: felt pen for signing fused work
What color does the silver sharpie fire to?Brad Walker wrote:Silver Sharpie won't burn off.
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Re: felt pen for signing fused work
Fuschia, of course . . .