Hi. Does anyone have a source of thick clear glass? need about 20 pieces about 6" x8" in either 1" or 1.5 inches thick. Can be float. Not cost effective to make, plus I don't want lines from sheet glass.
Thanks
Dick
thick glass
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: thick glass
There is 1" float, made somewhere offshore. I don't know a source. For 1.5", maybe you can get some Schott from HIS?
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: thick glass
Dalle de Verre glass is available from Kokomo in 8 x 12 x 1" in colors and clear
http://www.kog.com/more-glass/dalles.html
Tony
http://www.kog.com/more-glass/dalles.html
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Re: thick glass
thanks I will check it out
-
Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: thick glass
i've been fusing two pieces of 3/4 together to make 1.5" then cutting with a tile saw and fire polishing to achieve a thicker blank. You can see a fine line but it's not too noticeable.
Rick Wilton
-
williamslaybaugh
- Posts: 30
- Joined: Mon Mar 12, 2012 9:07 am
- Location: San Diego
Re: thick glass
I've got a bunch of the Dalle de Verre glass in storage. I'm not sure if I have 20 clear, but I also have transparent blue, green and red. I can run up there mid-week and post some photos and let you know what I've got if your interested.