How to make good seams

Post by Shelley Lewis »

This was my first attempt at making seams with different colored glass. I think I did pretty well for a first try, but when I hold the piece up to the light I can see a little light through the seams. I fused the three colors on top of a clear base. I think my cuts were good. Any suggestions or good techniques to share?
Attachments
image.jpg
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: How to make good seams

Post by Brad Walker »

Put the clear on top. The weight of the clear will help push the glass together and make the seams less likely.