recycling glass blocks

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
RobinH
Posts: 5
Joined: Sun Mar 02, 2014 12:40 am

recycling glass blocks

Post by RobinH »

I just tore out a glass block shower wall and now have a pile of this stuff...question, can I break up the glass and use it the same as float for creating shard glass bowls?
Has anyone and luck with this type of reclaimed glass?
I've also picked up some colored glass bowls at the Goodwill store. The plan was to throw them in the kiln just beyond full fuse to melt them down, then slump in a mold. Has anyone tried this, or am I wasting time with the reclaimed glass?
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: recycling glass blocks

Post by Brad Walker »

Glass blocks are usually mortared together. I don't know how easily that mortar can be removed. The glass itself may or may not be regular float -- some of the glass blocks are treated with other chemicals that may or may not work well in the kiln.

If you melt down the Goodwill bowls, don't try melting two different bowls together. They may be incompatible. They may also devitrify during the firing, so use a devitrification spray.

If you're interested in using up the glass block in a non-kiln way, check out this site: http://www.decobloc.com/home.asp
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: recycling glass blocks

Post by Judd »

OMG, too much drama. Use the glass as garden rocks, or... anything... Just don't bother melting it.
Post Reply