Frit balls with flat tops

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
lmartine
Posts: 36
Joined: Sat Mar 30, 2013 9:05 am

Frit balls with flat tops

Post by lmartine »

Hi,

What is the best way to make 1/8 inch thick frit balls with a flat top (in other words, I need oval-shaped, flattened 'balls'...):

1- Make the frit balls (full fuse) then flatten them under a KW-coated dam that will fall onto 1/8 inch fiber paper strips during a 2nd full fuse

or

2- Make the flattened balls in one full fuse step by placing my small glass pieces under the KW-coated dam held onto the fiber strips.

I know option #1 will work. I am just not sure whether the edges of the 1/8 inch thick glass pieces (i.e., those not in contact with the dam & the kiln shelf) would round up in option#2. Trying to save energy!

Cheers!

Lucie
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Frit balls with flat tops

Post by Morganica »

Cut long octagons (or hexagons) and fuse them, but stop the fuse before they draw up completely into balls?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Frit balls with flat tops

Post by Brad Walker »

Just curious -- after you make these flat-top balls, how will you use them?