Can I trim the edges of a finished piece using water jet ?
Moderators: Brad Walker, Tony Smith
-
Maggie Abdel Rahman
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
Can I trim the edges of a finished piece using water jet ?
Hello !
I have a question about trimming the edges of finished piece using water jet or laser cutting. I did fusing and slumping in one firing using a mold I constructed myselt. I cut the glass larger than the desired shape to leave about 3.5 cm of glass resting on the border for the glass to sag easily inside the mold without accumulating in the bottom. The result was OK , and now I want to trim the edges. If I use a simple glass cutter the result is not guaranteed. Can I do the trimming using water jet, or laser cutting at a specialized shop? Thanks to all !
I have a question about trimming the edges of finished piece using water jet or laser cutting. I did fusing and slumping in one firing using a mold I constructed myselt. I cut the glass larger than the desired shape to leave about 3.5 cm of glass resting on the border for the glass to sag easily inside the mold without accumulating in the bottom. The result was OK , and now I want to trim the edges. If I use a simple glass cutter the result is not guaranteed. Can I do the trimming using water jet, or laser cutting at a specialized shop? Thanks to all !
- Attachments
-
- slumped plate compressed.jpg (19 KiB) Viewed 22307 times
Re: Can I trim the edges of a finished piece using water jet
Most of us just use abrasives, either diamond or silicon carbide. If you've got a friend with a water jet, go for it.
-
Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: Can I trim the edges of a finished piece using water jet
It can work with a waterjet but will likely cost you $100 to get it done. (based on local waterjet pricing)
As MArty said abrasives is likely a better way to go, you can spend the cash on something that'll be useful for years to come.
As MArty said abrasives is likely a better way to go, you can spend the cash on something that'll be useful for years to come.
Rick Wilton
-
Mike Jordan
- Posts: 94
- Joined: Mon Nov 06, 2006 11:13 pm
- Location: Hillsboro, OR
- Contact:
Re: Can I trim the edges of a finished piece using water jet
Since it is straight edges, you might also consider finding someone that has a glass cutting bandsaw and trim the edges that way, then cold work the edges. Unless you use abrasives to polish, you will probably need to fire polish (in case you hadn't thought of that)... even a water jet cut would need cold working on the edges.
Mike
Mike
It's said that inside each of us is an artist trying to get out. Well mine got out... and I haven't seen him since.
-
Maggie Abdel Rahman
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
Re: Can I trim the edges of a finished piece using water jet
It is a paradox that not too many workshops in Egypt use bandsaws but more sophosticated machines are abundant because of the well established marble industry. What temperature would you suggest for fire polishing an already slumped piece? Should I keep it inside the original mold to avoid distortion?Mike Jordan wrote:Since it is straight edges, you might also consider finding someone that has a glass cutting bandsaw and trim the edges that way, then cold work the edges. Unless you use abrasives to polish, you will probably need to fire polish (in case you hadn't thought of that)... even a water jet cut would need cold working on the edges.
Mike
Re: Can I trim the edges of a finished piece using water jet
Yes, keep it in the original mold. Otherwise you will unslump it.
-
Maggie Abdel Rahman
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
Re: Can I trim the edges of a finished piece using water jet
Many thanks for your ideas. They were very helpful !
Re: Can I trim the edges of a finished piece using water jet
makes sense. I do recall that they've been cutting stone for a few years in that particular corner of the world.Maggie Abdel Rahman wrote:clip
because of the well established marble industry.
Re: Can I trim the edges of a finished piece using water jet
I think they copied Havi's pyramids, too.
Jen
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Can I trim the edges of a finished piece using water jet
The only issue I see is how you set the piece on the waterjet machine. The machine will cut plumb, relative to it's level base. Usually they put some solid throw away material beneath the glass that gets cut along with the glass. Your issue is to get the glass to sit stable and at the right angle. I have routinely cut thick fused glass on a waterjet machine.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Maggie Abdel Rahman
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
Re: Can I trim the edges of a finished piece using water jet
I think they (the workshop) will have to invert the piece and cut around the original shape or, as you mentioned, put some kind of support under the flat areas