Hand any one used photo decals from Fusion? http://www.fusionheadquarters.com/product_p/decpap.htm
It says"If your printer is a Black and White HP or Canon Laser Printer or copier and has absolutely NO capability of printing in color… it will work."
Thanks -
photo decals - black and white
Moderators: Brad Walker, Tony Smith
-
Terry Ow-Wing
- Posts: 124
- Joined: Sun Mar 09, 2003 3:21 pm
- Location: San Francisco, Ca.
- Contact:
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: photo decals - black and white
Best I can tell, this is the standard decal paper available in many places including our web store (see below).
Many canon printers do have the iron oxide in the toner, but some do not. You are pretty safe with HP black only printer
Note: you still get the "sepia" color, also known as rust.
Barry
Many canon printers do have the iron oxide in the toner, but some do not. You are pretty safe with HP black only printer
Note: you still get the "sepia" color, also known as rust.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
Terry Ow-Wing
- Posts: 124
- Joined: Sun Mar 09, 2003 3:21 pm
- Location: San Francisco, Ca.
- Contact:
Re: photo decals - black and white
thanks for the answer I just remember a ton of talk about which printers had the iron oxide and if there was enough .Barry Kaiser wrote:Best I can tell, this is the standard decal paper available in many places including our web store (see below).
Many canon printers do have the iron oxide in the toner, but some do not. You are pretty safe with HP black only printer
Note: you still get the "sepia" color, also known as rust.
Barry