kit to make wet lap sander

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Redfisher
Posts: 20
Joined: Sat Feb 26, 2005 12:03 pm
Location: St Augustine, FL

kit to make wet lap sander

Post by Redfisher »

I can't find it, but I could swear there was a kit to make a wet lap sander, that was talked about years ago her made from a tire... am I nuts or did I dream it?? :?
Help me please!!!! :wink:
Thanks in advance.
Terri
<'{{{{><
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: kit to make wet lap sander

Post by Rick Wilton »

His Glassworks has plans on their website to make one but I don't recall any kit. Others might

http://www.hisglassworks.com/files/lapplans.pdf
Rick Wilton
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: kit to make wet lap sander

Post by DonMcClennen »

Yes ... years ago a site member built one and posted many great photos of his excellent work. I think that person no longer posts here.
"The Glassman"
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: kit to make wet lap sander

Post by Brad Walker »

DonMcClennen wrote:Yes ... years ago a site member built one and posted many great photos of his excellent work. I think that person no longer posts here.
That person was probably Ron Coleman, who unfortunately passed away a couple of years ago. His old website is no longer online.
Redfisher
Posts: 20
Joined: Sat Feb 26, 2005 12:03 pm
Location: St Augustine, FL

Re: kit to make wet lap sander

Post by Redfisher »

Ok thanks guys!!
Terri
<'{{{{><
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: kit to make wet lap sander

Post by Marty »

If you use HIS' plans, consider not using the tire- if I ever re-do mine it'll be with brushes.
Redfisher
Posts: 20
Joined: Sat Feb 26, 2005 12:03 pm
Location: St Augustine, FL

Re: kit to make wet lap sander

Post by Redfisher »

With brushes?? What do you mean??
Did you use those plans?? Can you post a pic, of what you have, please??
Thanks for the tip!!
Terri
<'{{{{><
beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: kit to make wet lap sander

Post by beninfl »

If someone remembers his old website URL........ Go to http://web.archive.org and type it in there. You'll pull up old copies that they've archived for sites that go down just like this. It's like looking back in time. :-)
Redfisher
Posts: 20
Joined: Sat Feb 26, 2005 12:03 pm
Location: St Augustine, FL

Re: kit to make wet lap sander

Post by Redfisher »

Awesome... hope some remembers!
Terri
<'{{{{><
David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Re: kit to make wet lap sander

Post by David Jenkins »

I also made one (my own "plans"), and posted here about that experience. That was about 4 years ago, I think. I love my lap grinder, but if I were to build another here's some features I'd be sure to include this time:

1. Mine is 18" - I'd definitely go 24" next time
2. I'd spend the money on some slowing/stopping resistors
3. I would not spend extra money on variable speed motor control - I bet I use that less than 1% of the time, and I really don't need it then
4. Mine is made to work standing up. I might seriously consider lowering it so that I can work sitting down. Dunno - not real sure about that one, I guess.

Good luck with your project.
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: kit to make wet lap sander

Post by Marty »

Definitely 24", not worth bothering for less.
I use a stick for a brake (from underneath, not on the plate!)- cheaper than resistors.
Variable speed is needed if you'll be going to cerium.
Rather than lowering the machine, raise the operator. There are times I want to be close to eye level so I sit on something low. Sometimes I'm standing on a box so I can get leverage above the plate.

There was never a kit, just plans, and a photo of mine will add nothing to the plans. I do have a serious spray shield around the back, made out of corrugated plastic sheet, and there's a kitchen exhaust hood over the whole thing to keep the mist out of my face. Warm water!
The brushes are what comes with the Covington lap- they keep most of the spray in but let you run larger pieces off the wheel. The tire is good if you never plan on doing big stuff.

Any competent machinist should be able to take HIS plans and photos of the machines available and make you a great flat lap for less than half what the manufacturers charge.
When you start buying diamond pads for your new lap, you'll get what you pay for. Chinese plates are cheap, will have a wider size range of stone in the same plate (is that denier?) and won't last as long. I've stuck with HIS over the years.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: kit to make wet lap sander

Post by Brad Walker »

beninfl wrote:If someone remembers his old website URL........ Go to http://web.archive.org and type it in there. You'll pull up old copies that they've archived for sites that go down just like this. It's like looking back in time. :-)
Great suggestion. Not all of Ron's old site is online, but there is a folder with a lot of the information from the lap wheel he built. It's here: http://web.archive.org/web/200207050344 ... m/grinder/

Or go directly to a pdf with the design: http://web.archive.org/web/200306290908 ... rinder.pdf

Ron was an incredibly talented and generous person and was one of the first people to visit this board, going back to 2000. His fused glass boxes were magnificent (and totally fused, no glue): http://web.archive.org/web/200210221334 ... essel.html (I actually have a set of slides detailing Ron's process for making these boxes.)
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: kit to make wet lap sander

Post by charlie »

i built both ron's 24" flat lap and his blasting cabinet. i have the plans and parts list if anyone's interested.
Barry Gitelson
Posts: 31
Joined: Sat Feb 07, 2009 8:28 pm
Location: On the mountain side in Kona Hawaii

Re: kit to make wet lap sander

Post by Barry Gitelson »

That box Ron made is incredible. And how generous it was of him to share his techniques.
Barry Gitelson
Kona, HI

"Some dance to remember, some dance to forget" Hotel California - The Eagles

"Your talent is God's gift to you. What you do with it is your gift back to God." Author: Leo Buscaglia
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: kit to make wet lap sander

Post by Tony Smith »

Brad,

Will you pull these photos and the PDF off of the archive site and store them locally? It's rare that we get a chance to reach back and revisit history.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: kit to make wet lap sander

Post by Brad Walker »

Tony Smith wrote:Will you pull these photos and the PDF off of the archive site and store them locally? It's rare that we get a chance to reach back and revisit history.
I've pulled as much of Ron's information as I could off the archive site, except of course for his personal family photos. It's on my hard drive, along with some other photos and such that Ron sent me before he passed away. Perhaps I can put it together in some way to make it available to others.
Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: kit to make wet lap sander

Post by Georgia Novak »

Could someone please explain the firing rates. He lists "120 minutes - 1000f, 20 minutes 1000f, 60 minutes 1450f, 60 minutes 1450f, anneal 4 hrs @ 950f, 4 hrs to 750f, off. I don't understand the first four. Thanks, Georgia
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: kit to make wet lap sander

Post by Brad Walker »

Georgia Novak wrote:Could someone please explain the firing rates. He lists "120 minutes - 1000f, 20 minutes 1000f, 60 minutes 1450f, 60 minutes 1450f, anneal 4 hrs @ 950f, 4 hrs to 750f, off. I don't understand the first four. Thanks, Georgia
Take 120 minutes to get to 1000.

Then hold at 1000 for 20 minutes

Then take 60 minutes to get to 1450

Then hold at 1450 for 60 minutes

Some controllers use this method of entering the information instead of rates.
Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: kit to make wet lap sander

Post by Georgia Novak »

Thank you Brad. It went completely over my head. Georgia
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: kit to make wet lap sander

Post by Buttercup »

Following the link supplied by beninfl I searched for old WGB posts and found posts starting in 2000, and going till 2005 until I ran into 404 errors. Lots of good stuff there and I'll no doubt be poking about there when I should be doing other things.:

http://web.archive.org/web/200009260321 ... /config.pl

I was looking for a thread from 2008 about DIY glassworking tools and equipment which had quite a lot of activity. Maybe it's time to start a new one. Jen
Post Reply