Enamels on copper

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
vblue
Posts: 98
Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas

Enamels on copper

Post by vblue »

I have a bunch of FuseMaster lead free enamels.....all are in the 5000 group. Can these be used for copper enameling?

Thanks,
Vernelle
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Enamels on copper

Post by Brad Walker »

If they're the High Fire Lead Free Opaque enamels, they can be used for copper enameling. The Low Fire and Transparent are for glass only.
vblue
Posts: 98
Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas

Re: Enamels on copper

Post by vblue »

Thank you Brad.