I have a bunch of FuseMaster lead free enamels.....all are in the 5000 group.  Can these be used for copper enameling?
Thanks,
Vernelle
			
			
									
						
										
						Enamels on copper
Moderators: Brad Walker, Tony Smith
- 
				Brad Walker
 - Site Admin
 - Posts: 1537
 - Joined: Fri Mar 07, 2003 9:33 pm
 - Location: North Carolina, USA
 - Contact:
 
Re: Enamels on copper
If they're the High Fire Lead Free Opaque enamels, they can be used for copper enameling.  The Low Fire and Transparent are for glass only.
			
			
									
						
										
						Re: Enamels on copper
Thank you Brad.