Old, and I mean really old kiln wash?
I was gifted a huge bag/box of kiln wash, dated in the early 1970s....can anyone advise if this has a shelf life and might be trusted?  Thanks for any input!  ~ Missy
			
			
									
						
										
						- 
				rosanna gusler
 - Posts: 730
 - Joined: Mon Mar 10, 2003 2:22 pm
 - Location: wanchese north carolina
 - Contact:
 
Re: Old, and I mean really old kiln wash?
wash a piece of tile and fuse on that and see what happens. r.
			
			
									
						
							artist, owner of wanchese art studio, marine finisher
			
						- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
Re: Old, and I mean really old kiln wash?
It's probably as good as it was in the 70's if moisture hasn't turned it into a rock. That said, it was probably for ceramic or clay firing and I suspect the formula for glass firing might be a bit different. You'll have to try it and see.
Tony
			
			
									
						
							Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						- 
				Tom Fuhrman
 - Posts: 187
 - Joined: Mon Mar 10, 2003 11:44 am
 - Location: eastern Tennessee
 - Contact:
 
Re: Old, and I mean really old kiln wash?
should be OK, I'm still using some I got in the early 80's.