Kachina Bowls

Post by Babette (Shawn) »

Two new bowls, both are 22 inch diameter, system 96 glass. The turquoise and black one (lower bowl) has an irregular edge, made by placing 10 large powder wafers on top of 10 turquoise green slices of glass (shaped like pizza slices) Then those ten "slices" were placed on one large single layer of black glass. The black glass pulled up between the "slices" giving the piece a scalloped edge, no cold working. The brown and turquoise bowls was also made with powder wafers, with a cold worked edge,
Attachments
kachina bowl2.jpg
Kachina bowl 10.jpg
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: Kachina Bowls

Post by beninfl »

That's pretty pimpin!
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Kachina Bowls

Post by Valerie Adams »

Looks like you're having a lot of fun!
I especially appreciate you taking the 'basic' powder wafer concept and making it your own.
Joyce Walters
Posts: 80
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: Kachina Bowls

Post by Joyce Walters »

Thank you for sharing the photos of your wonderful work.
Your work always surprises, and inspires, and gives me great pleasure.
I remember the fish!
Joyce
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Kachina Bowls

Post by Don Burt »

Good stuff. Looks like they're in good company too.
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Kachina Bowls

Post by Sharol »

Shawn,

These are really great! I especially appreciate the way you work with the glass' inherent tendancy to pull up. Very cool and showcases your craftmanship and attention to detail. I like them both very much.

Keep going with this series!

Sharol
carol carson
Posts: 58
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Kachina Bowls

Post by carol carson »

Well Done! Really beautiful work.
Leonard Cichowski
Posts: 7
Joined: Wed May 15, 2013 9:29 pm
Location: Richmond, TX

Re: Kachina Bowls

Post by Leonard Cichowski »

Magnificent !!!!!!!
suds
Posts: 34
Joined: Fri May 09, 2014 10:44 pm
Location: Sonoma County, CA

Re: Kachina Bowls

Post by suds »

Beautiful plates! I especially like the "10 slice" one. Very fun!
What can you tell me about the brown glass that makes the background on the piece in the first photo? I love the cobblestone texture that it has.
Steve
osnat
Posts: 49
Joined: Wed Oct 21, 2009 10:02 pm
Location: Israel
Contact:

Re: Kachina Bowls

Post by osnat »

Hi Shawn

Beautfull works. I especially liked the second one
Osnat
Michele gh
Posts: 71
Joined: Tue Sep 21, 2004 11:10 pm
Location: Massachusetts
Contact:

Re: Kachina Bowls

Post by Michele gh »

exciting and distinctive work.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Kachina Bowls

Post by Buttercup »

Very complex and distinctive. I too, like the second one very much. Congratulations, Jen.
Babette (Shawn)
Posts: 103
Joined: Fri Feb 05, 2010 4:11 pm
Location: Chico California
Contact:

Re: Kachina Bowls

Post by Babette (Shawn) »

Thank you all for the positive feedback! It was much needed, I entered both of these bowls in a show last month and they were both rejected. I will keep plugging on!

-Shawn
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Nicole Hanna
Posts: 27
Joined: Wed Jul 27, 2005 10:17 am
Location: SW Missouri
Contact:

Re: Kachina Bowls

Post by Nicole Hanna »

Whoever rejected them didn't appreciate glass work....disregard their opinion and keep up the good work!

N.
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Kachina Bowls

Post by Buttercup »

Years ago, well back in last century, in another country, I was asked to enter a painting in the local show. I entered a quite passable oil of the head of an Arab stallion. It came second. A paint-by-numbers of The Last Supper came first. In retrospect, a rejection would have been a blessing. Jen