Re: vasoline glass
No hazards. The uranium oxide is totally contained.
Re: vasoline glass
My experiments were not pleasing. It fused like float.
-
Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: vasoline glass
Also, known as uranium glass, it's glass that is made with a small amount of uranium oxide. That makes it glow under a black light. It was really popular around the 30's, but stopped being widely made after WWII, when uranium was used for other things.Greg Rawls wrote:What is vasoline glass?
Today you mostly find it in some boro (for pipes) and marbles (glow in the dark). There was a company making some for fusing a few years ago, but I don't know if they're still around.
Called Vaseline glass because that's the color.