Post by G's »

Does anyone know if it is possible to turn my small Satellite J-100 jewelry kiln into a vitrigraph kiln? The top part is the interior of the kiln and the narrower bottom part is pretty empty and houses the element ends traveling to the temperature dial.
Thanks!
Ginny
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Making a Vitrigraph Kiln

Post by Brad Walker »

The Satellite J-100 is an $800 burnout kiln. Why not sell it to someone interested in enameling or small castings and use the money to buy a Hotsite/Hotbox/Caldera or similar kiln made for use with glass. The models sell for $400 to $600 new and would work much better than trying to convert the kiln you have.
Barbel
Posts: 17
Joined: Sat Dec 10, 2011 11:09 pm
Location: Ocean- Newport, North Carolina

Re: Making a Vitrigraph Kiln

Post by Barbel »

Love my Olympic Hotsie kiln!
I use it only as vitrigraph kiln, the new collar gives it more heighth than the Caldera has, all sorts of new options opening up!

Thank you, Brad for finding the collar for me, it is clicking along right now with a pot full of 'goodies'!
Barbel
G's
Posts: 29
Joined: Wed Nov 28, 2007 12:43 am
Location: Near Great Falls, Montana

Re: Making a Vitrigraph Kiln

Post by G's »

Huh. I didn't even think about that. Anybody want to buy a jewelry kiln?
S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: Making a Vitrigraph Kiln

Post by S.TImmerman »

G's wrote:Huh. I didn't even think about that. Anybody want to buy a jewelry kiln?
Try posting this is the "buy and sell" board here. make sure you list the model. price and age of kiln. Your location would be helpful too. I bought a paragon calandra along with 18''X18"X6' metal shelves for my set up. swapped out a kiln shelf and kaiser lee board for the bottom the kiln. I just bought an extra collar for this kiln to use taller pots. Its a great kiln for pulling cane.
Post Reply