I want to cut some mirror and cold work the edges. Anything I should know?
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: coldworking mirror--like regular glass?
The glass is regular float. The backing is regular paint.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: coldworking mirror--like regular glass?
I know that. will it behave any differently with wet belt/grinder?
Re: coldworking mirror--like regular glass?
no, except the silvering or paint may chip on the edges. use a very fine grit head on your grinder and belts.
Re: coldworking mirror--like regular glass?
Nina, I can hardly wait to see what you're doing with mirrors. I hope its nothing practical.
Vonon
Re: coldworking mirror--like regular glass?
let me reflect on a reply..
Re: coldworking mirror--like regular glass?
Nina, if you're bonding it to other glass or a substrate make sure you use an appropriate bonding agent. Some eat the silvering. Sorry I can't come up with a North American brand name right now but someone will know. Jen
Re: coldworking mirror--like regular glass?
it is far more humble..just for a base for my glass. I just want to customize the size/shape of the mirror.
Re: coldworking mirror--like regular glass?
FYI, scratching out a design on the backside of a mirror then slumping into shape produces interesting results. Often the paint comes off leaving the silver layer intact (my favorite tool for this is a razor blade). Modern day electro-plated mirrors react differently than old-time poured silver w/ bituminus applied paint. Fired mirror results often varies in color; pink, yellow, black - and I haven't been able to control that.
Re: coldworking mirror--like regular glass?
thanks for sharing your experiments, Mark!
Re: coldworking mirror--like regular glass?
Carefully controlled sandblasting will remove the paint if you can stop before removing the 'silvering'.
Mark, would there be any toxic fumes from the heated silvering? I just looked it up and the modern coating seems to be aluminum. How safe is that? Jen
Mark, would there be any toxic fumes from the heated silvering? I just looked it up and the modern coating seems to be aluminum. How safe is that? Jen
Re: coldworking mirror--like regular glass?
Safe? I'm more concerned about all the aluminum used in most deoderants, or cooking in aluminum pans than backs of mirrors!
Re: coldworking mirror--like regular glass?
The undisturbed aluminum on the items you mention won't enter your lungs. I'm not an expert, don't even have anything to base my question on other than evidence of the damage that other normally-inert substances can do if heated and inhaled. Being curious I Googled 'neurotoxicity of aluminum fumes'. Try it. Jen
Re: coldworking mirror--like regular glass?
I guess we're a bit off topic discussing warm working mirror instead of cold working, but it's all relevant to our trade. I did google toxicity of aluminum and there is some evidence it may be harmful but the jury is still out on this. However, I suspect many substrates we apply to glass then fire may be harmful to some degree. Burning off copper-plated backing or any kind of organic paint can't be good to breathe. I would certainly not want my kiln near my living quarters such as in the basement or attached garage. If in doubt, I'll start the program at the end of the day leaving the spiders to deal with the fumes. It's not something done regularly so it's not too different than all the other dangers we face every day.