Sand Mold question,
Moderators: Brad Walker, Tony Smith
- 
				jim burchett
 - Posts: 255
 - Joined: Sun Jun 29, 2003 4:24 pm
 - Location: Lenoir, NC
 
Sand Mold question,
I have made a Box Sand Mold and have Pressed textures into the sand to make relief in the glass. I am wondering if I sift powders into the depressed areas of the mold and then take it to a Tack fuse temp if the powders will provide contrast to those areas?
			
			
									
						
							"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
			
						- 
				rosanna gusler
 - Posts: 730
 - Joined: Mon Mar 10, 2003 2:22 pm
 - Location: wanchese north carolina
 - Contact:
 
Re: Sand Mold question,
Probably. The Fritz might ball up before the other glass touches dowm though
			
			
									
						
							artist, owner of wanchese art studio, marine finisher
			
						- 
				jim burchett
 - Posts: 255
 - Joined: Sun Jun 29, 2003 4:24 pm
 - Location: Lenoir, NC
 
Re: Sand Mold question,
Well its worth a try...long slump at 1225 then quick up to 1400..will let you know how it works out.
			
			
									
						
							"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie