Hello. Does anyone know at what temperature wax completely carbonises?
Pete
Wax carbonisation temp?
Moderator: Brad Walker
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Wax carbonisation temp?
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Wax carbonisation temp?
You trying to burn wax and any organic contaminants completely out of the mold? That's around 800C.Peter Angel wrote:Hello. Does anyone know at what temperature wax completely carbonises?
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Wax carbonisation temp?
I'm steaming out the wax beforehand but there's always a tiny bit of wax residue.
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.