Sounds silly but can I put a picture inbetween two pieces of glass. Would it burn out? or worse cause a fire?
Thank you. Raphy
paper between two sheets of glass
Moderator: Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: paper between two sheets of glass
To burn it needs oxygen. Without oxygen it will become charcoal. With oxygen it will become fire.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: paper between two sheets of glass
The organics will usually burn out in the kiln and may or may not leave a bit of ash behind--most layups aren't airtight and at burnout temps (600-700F) the glass hasn't yet softened and sealed in/out air. The real question is, though, what else the paper leaves behind. Some inks can stain the glass or leave a residue, and some types of paper have clay or other coatings that can also leave residue.
Also depends on how much you're using. A postage stamp-sized piece of blank cheap newsprint probably won't do much. A big piece of glossy cardstock with a photograph and text printed on both sides might. Some of the inks might stain the glass and cause a visible reaction; others won't, so you might or might not get a nice result.
If it causes a fire, it's in a kiln, which is a pretty fireproof place. I wouldn't worry unless you're burning something like the Sunday New York Times and the flames start to lick out of the vents. There is a chance that combustion could be fast enough to jolt the glass and cause it to shift position but again, you'd need a bunch of paper relative to the amount of glass.
If you're trying to fuse a photograph into glass and have it look like a photograph, search this site for "screen printing," "photo transfers," and "print-making." You'll find a fair amount of information on how to get images into glass. The folks who own this site have written a book about these techniques that's worth a look.
Also depends on how much you're using. A postage stamp-sized piece of blank cheap newsprint probably won't do much. A big piece of glossy cardstock with a photograph and text printed on both sides might. Some of the inks might stain the glass and cause a visible reaction; others won't, so you might or might not get a nice result.
If it causes a fire, it's in a kiln, which is a pretty fireproof place. I wouldn't worry unless you're burning something like the Sunday New York Times and the flames start to lick out of the vents. There is a chance that combustion could be fast enough to jolt the glass and cause it to shift position but again, you'd need a bunch of paper relative to the amount of glass.
If you're trying to fuse a photograph into glass and have it look like a photograph, search this site for "screen printing," "photo transfers," and "print-making." You'll find a fair amount of information on how to get images into glass. The folks who own this site have written a book about these techniques that's worth a look.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: paper between two sheets of glass
I have to laugh, Cynthia. Many years ago, my girlfriend was a novice jeweler. She decided to make a silver casting of a tiny plastic moose. She used the lost, little plastic moose method, of casting. She invested it with sprues and stuck it in the kiln. A fire ensued that almost killed the elements in the kiln. I have had and loved the silver moose for 30 some years. That was the last time she employed the technique...
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: paper between two sheets of glass
I've taken a piece of BE thin fire did a small drawing with pencil and placed it between a base of black and clear top and it turned out fine.
Re: paper between two sheets of glass
...and then there's leaving a layer of graphite between the glass...AndyT wrote:I've taken a piece of BE thin fire did a small drawing with pencil and placed it between a base of black and clear top and it turned out fine.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: paper between two sheets of glass
You could try putting kiln paper (eg bullseye thinfire) between 2 sheets of glass and fuse all that together.
I have no idea what might happen.
Pete
I have no idea what might happen.
Pete
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Re: paper between two sheets of glass
Glass line sells a line of colored papers that are ment to be fired between sheets of glass. Guess what it's made of?? Thin fire!!!