Is the stand needed to provide ventilation to the underside of the kiln, or can I use it without the stand as long as it is on a fireproof surface? With the provided stand, it is too high up for me to see into. Thanks for any advice!
--jodi
Can I use Skutt Firebox 14 without a stand?
Moderators: Brad Walker, Tony Smith
-
Jodi Longobardo
- Posts: 34
- Joined: Sat Sep 30, 2006 7:51 pm
- Location: NJ
Re: Can I use Skutt Firebox 14 without a stand?
you can use any kiln as long as it's on something fireproof, or open to the air. there's nothing special about a stand.
-
Jodi Longobardo
- Posts: 34
- Joined: Sat Sep 30, 2006 7:51 pm
- Location: NJ
Re: Can I use Skutt Firebox 14 without a stand?
Thanks, Charlie!
--jodi
--jodi
Re: Can I use Skutt Firebox 14 without a stand?
Is there a warranty involved? Not using the provided stand might void some warranty. Calling the manufacturer for guidance would probably be prudent.
Jerry