Post by Anne-Claire »

Here is my first post, a 9 mm Bullseye glass plate :
3 mm black, 6 mm clear, white and red stripes and a window made of puddles (thanks to Paul Tarlow's puddles tutorial).
It was fun to make it, I hope you'll enjoy the pictures.

I'd like to thank you all for the advice, information and discussions one can find in this forum. They were really helpful for me.
anne-claire
plat.JPG
window.jpg
detail-window.jpg
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Black plate with a red puddles window

Post by Don Burt »

Handsome plate Anne-Claire. Congratulations
Jeanice
Posts: 35
Joined: Sun Jan 01, 2012 1:24 pm
Location: Wyoming, USA

Re: Black plate with a red puddles window

Post by Jeanice »

Very nice!
Jeanice
Drewcilla
Posts: 60
Joined: Fri Apr 11, 2008 9:10 am

Re: Black plate with a red puddles window

Post by Drewcilla »

Nice work. Thanks for sharing.
Haydo
Posts: 292
Joined: Fri Mar 14, 2003 9:55 am
Location: Eimeo, Qld., Australia
Contact:

Re: Black plate with a red puddles window

Post by Haydo »

BINGO. ...bring me another drink o......nearly rhymes damn it.
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Black plate with a red puddles window

Post by Vonon »

A very striking design and well executed. A special achievement keeping the long red and white lines that angle across the plate so straight.
Vonon
Anne-Claire
Posts: 2
Joined: Fri Oct 18, 2013 8:32 pm
Location: Massy (near Orly Airport, France)

Re: Black plate with a red puddles window

Post by Anne-Claire »

Vonon, the lines are 6mm wide Bullseye stripes, on the edge. Forgot to mention the clear glass is on top of the black one, so we see the stripes from top and side.

Thank you so much for your kind comments.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Black plate with a red puddles window

Post by Havi »

Beautiful!!!

Havi

Where can I find Paul Tarlow's puddles tutorial???

Thanks,
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
linn keller
Posts: 52
Joined: Mon Mar 10, 2003 12:22 pm
Location: south tx

Re: Black plate with a red puddles window

Post by linn keller »

Havi,
You'll find the puddles tutorial and a tremendous bunch more stuff on Paul's site here:

fusedglass.org

Linn
linn in deep deep south texas
KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: Black plate with a red puddles window

Post by KaCe »

Thank you for posting this. I love your work. It is exactly my color pallet... I love black, red and white. I am going to have to read that tutorial that inspired you. Perhaps I can get good results, too. Thank you again for sharing your lovely work.
KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: Black plate with a red puddles window

Post by KaCe »

I did a search for Paul Tarlow's puddles and found nothing here. Where did you find it? TIA
Jeanice
Posts: 35
Joined: Sun Jan 01, 2012 1:24 pm
Location: Wyoming, USA

Re: Black plate with a red puddles window

Post by Jeanice »

Go to fusedglass.org. Learn > Project Tutorials. I think you will like the other tutorials too.
Jeanice
KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: Black plate with a red puddles window

Post by KaCe »

Thank you for the link to the tutorials. I am excited to experiment. I loved the "puddles" and also the "pressed glass"tutorials. I will be trying these out this fall.I will post my efforts when completed. Thank you again.
Post Reply