Hello all,
Question. Is it better to pre fire a blank ie 2 3mm clears together first before setting it on the fibre paper or can the the two blanks be fired over the paper in one step? Also, does anyone have a fool proof schedule for both 96 and bullseye getting fine details?
Thanks in advance,
Peter
Kiln carving question
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Kiln carving question
I kiln carve float. My advice would be to do a single firing with a good bubble squeeze. Simply fire hot enough to get the edge you like, and the kiln carving will take care of itself.
When I kilncarve float, I prefer to fire lower and slower than most others.
When I kilncarve float, I prefer to fire lower and slower than most others.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions