BE Opaline Striker
Moderators: Brad Walker, Tony Smith
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
BE Opaline Striker
Tried to put opaline striker over BE turquoise and it has turned brown. Have not read anything that suggested it was reactive........Any suggestions?
Thanks, Barbara Hale Elmore
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Re: BE Opaline Striker
Pics, please? Are we talking frit, sheet..?
It's not supposed to contain copper-reactive stuff (sulfur/selenium/lead)...so are you sure it's opaline striker? Could it possibly be reactive cloud opal or translucent white? Both of those look sorta like opaline in the raw state and they definitely will react...
It's not supposed to contain copper-reactive stuff (sulfur/selenium/lead)...so are you sure it's opaline striker? Could it possibly be reactive cloud opal or translucent white? Both of those look sorta like opaline in the raw state and they definitely will react...
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
Re: BE Opaline Striker
Sheet. Definitely opaline striker. The only thing I can think of is maybe my kiln temp is off from the 1490 suggested top temp. I am refining one piece as a test tonight.
Thanks, Barbara Hale Elmore
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
Re: BE Opaline Striker
Test piece came out from second firing (in a different kiln) just the same as first, dark, dark chocolate brown over the turquoise opal. Stumped.
Thanks, Barbara Hale Elmore
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
-
Warren Weiss
- Posts: 137
- Joined: Thu Mar 13, 2003 8:06 pm
- Location: Richmond, VA
Re: BE Opaline Striker
Barbara,
Ask Bullseye on their website.
Warren
Ask Bullseye on their website.
Warren
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
Re: BE Opaline Striker
Thanks, Warren, I posted it on their site and will contact Amy Ferber when she returns to portland.
Thanks, Barbara Hale Elmore
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Re: BE Opaline Striker
Hmmm. If you have a piece left over, try firing it on its own, without the turquoise. This one's really got me going.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
Re: BE Opaline Striker
OK!
Thanks, Barbara Hale Elmore
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb