Any experience using BE molds 8919 or 8920?

Post by David Jenkins »

Have you used either of these? Easy slump? Or difficult? Got a picture of the final product?

Thanks!
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Babette (Shawn)
Posts: 103
Joined: Fri Feb 05, 2010 4:11 pm
Location: Chico California
Contact:

Re: Any experience using BE molds 8919 or 8920?

Post by Babette (Shawn) »

It would help if you posted a photo of the molds.
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Re: Any experience using BE molds 8919 or 8920?

Post by David Jenkins »

Here ya go:
8919.jpg
8920.jpg
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Any experience using BE molds 8919 or 8920?

Post by Valerie Adams »

I haven't used them but Bullseye recently released a new Quick Tip: Suggested Slumping Schedules. It lists suggested slumping schedules for all their molds.
molds.jpg
molds.jpg (28.4 KiB) Viewed 9859 times
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Any experience using BE molds 8919 or 8920?

Post by DonMcClennen »

I've had those molds for about 15yrs. They are an easy slump.. just use Bullseye suggested schedule.
"The Glassman"
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Any experience using BE molds 8919 or 8920?

Post by JestersBaubles »

Check out the latest tip sheet from Bullseye:

http://www.bullseyeglass.com/images/sto ... dule_F.pdf

Dana
David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Re: Any experience using BE molds 8919 or 8920?

Post by David Jenkins »

@Dana:

Those tips are great help - thanks. Besides giving guidance for slumping a new mold, they allow me to parity check my schedules I've worked out independently over the last 5 years or so.
Dave Jenkins
Glass at Harbor Gates
Cypress, TX