Tac fuse for pebbles
Moderator: Tony Smith
Tac fuse for pebbles
I remembered from something that I cover a circle with pebbles then tac and slump. I have one layer circle and covered it with pebbles. Need suggestions for firing schedule - I don't want to loose the texture but I want the pebbles to most definately be attached. Thanks
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Tac fuse for pebbles
wont work. glass will break on cool dowd. r.
artist, owner of wanchese art studio, marine finisher
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Tac fuse for pebbles
Glass pebbles or rock pebbles?
Glass will work, rocks will not.
Jim
Glass will work, rocks will not.
Jim
-
Charlotte Kay
- Posts: 15
- Joined: Sat Dec 12, 2009 10:43 pm
- Location: Northern California
Re: Tac fuse for pebbles
I think she means fused glass "pebbles" that you make from breaking up a pattern bar or pot melt. Kinda like frit balls.
I have used either the 2-layer or the 3-layer fusing schedules for a tack fuse on fusedglass.org Depends on how thick your base circle is and how thick your pebbles are. You want to use the thickest measurement in your calculations.
I have used either the 2-layer or the 3-layer fusing schedules for a tack fuse on fusedglass.org Depends on how thick your base circle is and how thick your pebbles are. You want to use the thickest measurement in your calculations.
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact: