Small piece of frit casting mold chipped-can it be salvaged?
Apparently I didn't get enough mr97 on my brand new flower frit casting mold, and when I removed the fused glass a piece of the mold chipped off. Is there any way to salvage the mold, such as trying to smooth it with fine grit sand paper?
			
			
									
						
										
						Re: Small piece of frit casting mold chipped-can it be salva
Yes, you can definitely smooth it out. Remember, though, that you're working in negative space, so you're going to get a bumpout in the glass to match the hole. I'd try a firing with the chip as-is first, see if you like the result, and then potentially alter the mold with a fine diamond file or something similar when you know how it needs to change.
			
			
									
						
							Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
			
						Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
- 
				Shelley Lewis
- Posts: 73
- Joined: Wed Dec 11, 2013 11:14 am
Re: Small piece of frit casting mold chipped-can it be salva
Thank you, I'll give it a try!Morganica wrote:Yes, you can definitely smooth it out. Remember, though, that you're working in negative space, so you're going to get a bumpout in the glass to match the hole. I'd try a firing with the chip as-is first, see if you like the result, and then potentially alter the mold with a fine diamond file or something similar when you know how it needs to change.
- 
				jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Small piece of frit casting mold chipped-can it be salva
As a last resort, you can take a demel and make 3 or more coresponding "chips" on the mold.
I'll bet nobody has a mold like that :>)
Jim
			
			
									
						
										
						I'll bet nobody has a mold like that :>)
Jim