I was looking at Bullseye reactive glass chart. I'm not sure I'm reading it correctly.

Can you get reactions from any of the transparent glasses? Most of those listed say "opal".

Thanks,
Vernelle
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: reading BE reactive chart

Post by jim burchett »

The chart is pretty clear..you get reactions from the glasses listed..if it says opal then opal is where the reaction is
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: reading BE reactive chart

Post by Morganica »

Make sure you're looking at the latest version: http://www.bullseyeglass.com/images/sto ... _glass.pdf

The older versions used to list the transparent and opal glasses separately. The new chart mixes them up.

Opal glasses will have a 0 in the 4th from last position in the product number, as in "000208." Transparent glasses will have a 1 in that position, as in "001818."