Sand corner of mold?

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Susanbuckler
Posts: 68
Joined: Tue Aug 18, 2009 10:31 pm

Sand corner of mold?

Post by Susanbuckler »

Happy holidays to all
Finally have time to get back into my studio and I noticed a couple of the corners on BE molds are deteriorating slightly. Would you recommend sanding them a bit to even it out and then reapplying kiln wash ? Can I reapply kiln wash just to those spots or should I reapply it to the entire mold?
Thanks
Susan
Susan Buckler
Woodstock, NY
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Sand corner of mold?

Post by Vonon »

I have done both of those things with no problem. Sometimes have managed to chip a little kiln wash off the rim and just repaired it with a dab of fresh kw and smoothed it with my finger. I guess it depends on how fanatic you might be about a smooth backside. :wink:
Vonon