My latest deep slump vessel

Post by Babette (Shawn) »

This piece was done with stringers and frit and one piece of steel blue sheet glass. If you look at the rim you can see the steel color.
Attachments
image.jpg
image.jpg
Last edited by Babette (Shawn) on Fri Jan 02, 2015 10:26 pm, edited 2 times in total.
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: My latest deep slump vessel

Post by Warren Weiss »

Babette,
That is a lovely bowl! How deep is it? Was it done in a single slump or using the "3 bowl" slump technique? Thanks.

Warren
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: My latest deep slump vessel

Post by twin vision glass »

Oh so fantastic and beautiful and well, totally inspiring! Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Babette (Shawn)
Posts: 103
Joined: Fri Feb 05, 2010 4:11 pm
Location: Chico California
Contact:

Re: My latest deep slump vessel

Post by Babette (Shawn) »

I used the deep slump bowl #2 and #3, I started with a 20 inch disc, slumped into my old stainless steel sink mold for the first slump so in total it was slumped 3 times. The finished bowl is 9 inches deep and an inch thick, lots of glass!
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: My latest deep slump vessel

Post by Warren Weiss »

Babette,
Thanks. That is quite a statement in glass. Worth every pound of it!

Warren
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: My latest deep slump vessel

Post by Buttercup »

Well done, Shawn!