Can anyone help me with a mud-mixing problem I'm having with potmelts.
I am using an 8" diameter flowerpot with a 7/8" aperture. After stacking equal quantites of Bullseye Emerald Green (transparent) and Canary Yellow (opaque) vertically in the pot (green then yellow then green and so on) I end up with a horrible brown mixed up mess.
Are there only certain colour combinations that work? Or should I be adding the colours to the pot in thicker layers (I only layered one thickness of green then one of yellow etc)?
I'm trying to achieve results similar to Steve Immerman on his website (clearwaterglass.com) but to no avail - so far.
For info the firing cycle I used is 932 degrees F to 934 held for 60 mins then full rate to 1700 held for 2 hours (the pot completely emptied), then full back down to 934 again for 60 mins then 176 to cool.
Any help offered would be gratefully received.
Thanks