I am in the market for a Bell Style Kiln and am looking for some insights/experience others have had with this style of kiln and manufacturers and any input on who I should order one from.  I have quote requests in to Denver, Paragon and Olympic.  
Interior 40 x 17 x 18" deep, 220V, 3 Phase with an automatic Vent System, with a shelf, Overhead crane system w/roll out table and floor rail/docking system, and controller.
I'm in northern Washington state.
I already have a Paragon Pearl56 and GL24, but need a wider and longer shelf and taller kiln for fusing larger pieces and the occasional 1 - 2" thick table pieces.
Thanks for any advice/input you can offer.
			
			
									
						
										
						Which Bell Style Kiln would you recommend?
Moderators: Brad Walker, Tony Smith
- 
				Mary Simmons
- Posts: 2
- Joined: Thu Mar 28, 2013 7:37 am
- 
				Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: Which Bell Style Kiln would you recommend?
Euclids makes some great kiln. They are made in Canada and with our dollar taking a hit lately you'll likely save a significant amount.
http://www.euclids.com/index.php?cat_na ... tric-kilns
			
			
									
						
							http://www.euclids.com/index.php?cat_na ... tric-kilns
Rick Wilton
			
						- 
				Mary Simmons
- Posts: 2
- Joined: Thu Mar 28, 2013 7:37 am
Re: Which Bell Style Kiln would you recommend?
Thanks for the info.  I just sent them a quote request.
			
			
									
						
										
						- 
				Babette (Shawn)
- Posts: 103
- Joined: Fri Feb 05, 2010 4:11 pm
- Location: Chico California
- Contact:
Re: Which Bell Style Kiln would you recommend?
I like the Denver kilns, I bought mine used (10plus years old) and have used it almost every day for 2 years now, it has been great. My Denver is 40 long  by 25 inches wide, about 24 inches deep without the shelf, I have separate controllers for top elements and the side elements. I personally would like a wider kiln than 17 inches...I like to use the whole width of a sheet of glass. Check with Denver Kilns, they are very helpful,.
			
			
									
						
							“Art washes away from the soul the dust of everyday life.” 
― Pablo Picasso
			
						― Pablo Picasso
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Which Bell Style Kiln would you recommend?
I think bell style kilns are the best design.  However I don't like any manufactured designs I have seen, so I build my own.  First of all, the last thing i want to do, after I do a sensitive setup, is roll my floor.  My floors are stationary, the bell lifts up and rolls out of the way.  I think fiber blanket is a lousy hot face material.  I prefer using HD fiber boards. They are far more durable.  Denver under insulates their kilns. This makes them cheap to build.  They run really hot to the touch.  
There is no such thing as 220v 3 phase. Common wirings are 240v single phase, 208v single phase (derived from 3 phase) or 480v 3 phase. These are all really different, and require different designs. Heating elements don't really care about phase, only watts.
I am working on some new designs for embedding elements in fiber boards, and for being able to double production speed. These will take quite some time before I perfect them.
			
			
									
						
							There is no such thing as 220v 3 phase. Common wirings are 240v single phase, 208v single phase (derived from 3 phase) or 480v 3 phase. These are all really different, and require different designs. Heating elements don't really care about phase, only watts.
I am working on some new designs for embedding elements in fiber boards, and for being able to double production speed. These will take quite some time before I perfect them.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions