I purchased a 15" x12" x 2.5" medium wave mold. I have a piece that has the rounded edges from a full fuse.
Will the curvature of the slump allow the piece to stand on edge or will I need to cold work the edges?
Anyone have experience with this type of mold?
Thank you,
Vernelle
Wave mold
Moderators: Brad Walker, Tony Smith
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Wave mold
If the edge is straight to begin with (and squared), and you place it properly (completely straight/squared) on the mold, it will stand on its own. It will, however, be more stable if you coldwork the edge flat.
Dana W.
Dana W.
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: Wave mold
Agree with Dana. I always square mine off to get the additional stability. I would only add that a lap grinder makes quick and easy work of squaring off that edge. Doing it by hand might entail an awful lot of labor ...
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Glass at Harbor Gates
Cypress, TX
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
Re: Wave mold
I use my glass tile saw to get a nice straight edge. Easy!
Thanks, Barbara Hale Elmore
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Re: Wave mold
Thank you all for your answers. I teach fusing at a not-for-profit glass school here in Fort Worth and can use their equipment......lap grinder, saw, wet belt sander.... So I will be cold working the piece.
Thanks again for your help,
Vernelle
Thanks again for your help,
Vernelle
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
-
Barbara Elmore
- Posts: 19
- Joined: Wed Nov 19, 2003 5:47 pm
- Location: State Road NC
Re: Wave mold
Sawing is much easier before the slump, and when I get a nice, flat edge, I do not do any coldworking.
Thanks, Barbara Hale Elmore