I'm looking for advice on a good digital pyrometer to buy for my newly acquired used Paragon kiln.  Its is a manual control Paragon E14A model, with a Kiln-Sitter model LT-3 attached.  The kiln came with an analog pyrometer.  This is my first kiln, and now that I'm forging out of workshop-lead fusing I'd like to understand the equipment and move beyond "novice" with using it myself.
I'd prefer to get a digital pyrometer that I can connect to a PC and run some experiments to see what the "1" or the "3" on the control dial equates to before I start firing glass.  I can't figure out where to start in searching for a pyrometer - so many options.  Can anyone suggest some specifics for a single thermocouple digital pyrometer?  Thank you!!
			
			
									
						
										
						Need advice - digital pyrometer make/model
Moderator: Tony Smith
- 
				Stephen Richard
 - Posts: 302
 - Joined: Sun Jul 06, 2003 4:36 pm
 - Location: Glasgow, Scotland
 - Contact:
 
Re: Need advice - digital pyrometer make/model
If it were me, i would invest in an inexpensive controller.  You can hook the pyrometer to it and combine digital output as well as a means to control your segments without bothering to know what 1, 3, or 9 do.  Just set the rheostat to maximum and let the controller do the rest.
Yes, you will learn a lot about how glass performs at different temperatures and in different conditions (as I did), but it seems to me wasted time that could be spent on learning about your glass combinations.
			
			
									
						
							Yes, you will learn a lot about how glass performs at different temperatures and in different conditions (as I did), but it seems to me wasted time that could be spent on learning about your glass combinations.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
			
						You can view my Blog at: http://verrier-glass.blogspot.com/
- 
				Stephen Richard
 - Posts: 302
 - Joined: Sun Jul 06, 2003 4:36 pm
 - Location: Glasgow, Scotland
 - Contact:
 
Re: Need advice - digital pyrometer make/model
If it were me, i would invest in an inexpensive controller.  You can hook the pyrometer to it and combine digital output as well as a means to control your segments without bothering to know what 1, 3, or 9 do.  Just set the rheostat to maximum and let the controller do the rest.
Yes, you will learn a lot about how glass performs at different temperatures and in different conditions (as I did), but it seems to me wasted time that could be spent on learning about your glass combinations.
			
			
									
						
							Yes, you will learn a lot about how glass performs at different temperatures and in different conditions (as I did), but it seems to me wasted time that could be spent on learning about your glass combinations.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
			
						You can view my Blog at: http://verrier-glass.blogspot.com/
- 
				Rick Wilton
 - Posts: 273
 - Joined: Sat Oct 25, 2003 8:18 pm
 - Location: Calgary, Canada
 - Contact:
 
Re: Need advice - digital pyrometer make/model
Many cheap multi-meters work as pyrometers also.
this one from harborfreight $24.00 http://www.harborfreight.com/ac-dc-digi ... 37772.html

comes with a a temperature probe, this probe won't standup to kiln temps but you can easily change it to any type k thermocouples.
			
			
									
						
							this one from harborfreight $24.00 http://www.harborfreight.com/ac-dc-digi ... 37772.html

comes with a a temperature probe, this probe won't standup to kiln temps but you can easily change it to any type k thermocouples.
Rick Wilton
			
						- 
				Kevin Midgley
 - Posts: 773
 - Joined: Mon Mar 10, 2003 11:36 am
 - Location: Tofino, British Columbia, Canada
 
Re: Need advice - digital pyrometer make/model
These work.
http://www.digitry.com/index.html
Cheaper but won't be as simple to hook up.
Plus note the pricing is in Cdn$ currently at about 20% discount to the US$, making things incredibly cheap for those with US dolllars.
http://stores.ebay.ca/rogersdini?_trksid=p2047675.l2563
			
			
									
						
										
						http://www.digitry.com/index.html
Cheaper but won't be as simple to hook up.