Hello ! Is it possible to make "Pebbles" yourself ? If yes....different diameters ? Thank you for your help ! Jan
Re: "Pebbles"....making yourself ?
"Pebbles" are also called nuggets. Here is link to a previous post about making them...
http://www.warmglass.com/phpBB/viewtopi ... ts#p240202
http://www.warmglass.com/phpBB/viewtopi ... ts#p240202
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: "Pebbles"....making yourself ?
Thank you Jenna ! I did not know they were called nuggets too
Jan de Jong
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: "Pebbles"....making yourself ?
Hello, the link is not working anymore ?? Not so clever, forgot to archive the schedule. JanJenna wrote:"Pebbles" are also called nuggets. Here is link to a previous post about making them...
http://www.warmglass.com/phpBB/viewtopi ... ts#p240202
Re: "Pebbles"....making yourself ?
You can make nuggets/pebbles from any glass you have on hand and in any size you wish... pretty much.
I think the choice of separator must be important since I've seen so much discussion about cleaning the bottoms.
'Back in the day' I just put a piece or a small stack of pieces on the shelf & fired to the look I wanted - maybe 1300°F? I used kiln wash I got from a potter friend.
Here's a link you might enjoy: http://fusedglass.org/learn/project_tut ... ss_puddles
Have fun - experiment!
I think the choice of separator must be important since I've seen so much discussion about cleaning the bottoms.
'Back in the day' I just put a piece or a small stack of pieces on the shelf & fired to the look I wanted - maybe 1300°F? I used kiln wash I got from a potter friend.
Here's a link you might enjoy: http://fusedglass.org/learn/project_tut ... ss_puddles
Have fun - experiment!
please visit Beall Glass Studio on Face Book
-
De Anza Art Glass Club
- Posts: 21
- Joined: Wed Jun 09, 2010 10:12 pm
Re: "Pebbles"....making yourself ?
Bullseye's fit ball project sheet gives some information that might be helpful with larger balls/nuggets/pebbles:
http://www.bullseyeglass.com/methods-id ... balls.html
http://www.bullseyeglass.com/methods-id ... balls.html