Hello all, I just peeked into my kiln at a beautiful 14" bowl and noticed that one of the edges has a scalloped raised edge. The kiln is at 600 and coming down. It already annealed for two hours. I'm not going to like this ripple. Can I just start now and go ahead and run it through the slumping schedule again or do I have to wait until it is 100 degrees and fuse flat again and re slump? My instincts are saying to just re slump now...
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: RE-slumping

Post by Brad Walker »

You can just start now and re-slump.