New Alchemy / Silver Experiements

Post by twin vision glass »

I am having a wonderful time playing with the new Alchemy glass and have been amazed at all the possibilities and cannot sleep because I am so excited. Each layer is a different reaction all the way from Deep bronze to purple to a soft gold and silver ( best results with the 1401 crystal clear for soft gold look) . This experiment is 24 inchs wide and pushes the limits of my kiln and my deep Mold Mix 6 mold I made so I hope it works in the slump that is happening now. [-o<
phpYh7hTRPM.jpg
phpseramePM.jpg
phpUk3Yw3PM.jpg
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

The silver chemical transformation of colours look so different when put with different base colours and colours under and over. I have a birds nest also that just fired and the chemistry of the Alchemy with the silver is so exciting.
phpaZP22uPM.jpg
phpVp5We8PM.jpg
( this piece slumped nicely and will try to get a pic of it)
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: New Alchemy / Silver Experiements

Post by JestersBaubles »

Beautiful as always :)

Dana W.
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

Well I will for sure get a better picture as the piece is quite interesting and the light plays with all sorts of parts of this vessel, so stay tuned
phpbURbj0PM.jpg
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

phpBV0SLtAM.jpg
phpBV0SLtAM.jpg (50.42 KiB) Viewed 252859 times
phpgVXyVCAM.jpg
phpgVXyVCAM.jpg (59.9 KiB) Viewed 252859 times
php6l1ItBAM.jpg
php6l1ItBAM.jpg (52.29 KiB) Viewed 252859 times
I have been playing a lot with the new Alchemy glass and am really enjoying the different reactions one can get and when deep slump, the silver is stretched and torn and gives some really interesting affects
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

The other bowl slumped nicely too!
phpGa1BEQAM.jpg
phpGa1BEQAM.jpg (52.53 KiB) Viewed 252857 times
php5fKmPPAM.jpg
php5fKmPPAM.jpg (54.83 KiB) Viewed 252857 times
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

phpJPAoi4PM.jpg
phpJPAoi4PM.jpg (48.37 KiB) Viewed 252838 times
Forgot to show the underside of bowl with a lot of the Alchemy silver
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

phpNnIP2JPM.jpg
phpNnIP2JPM.jpg (48.61 KiB) Viewed 252831 times
php7Sf6P6PM.jpg
php7Sf6P6PM.jpg (46.96 KiB) Viewed 252831 times
phppAmYSwPM.jpg
phppAmYSwPM.jpg (45.19 KiB) Viewed 252831 times
Working on a silver and French Vanilla fumed large deep slump vessel also which will be really interesting as the outside will look so very different from the inside. Will try to get a photo when done but will take a few weeks to finish all slumps.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

phpLktIYjAM.jpg
phpLktIYjAM.jpg (50.54 KiB) Viewed 252798 times
phpPiTJ3RAM.jpg
phpPiTJ3RAM.jpg (53.2 KiB) Viewed 252798 times
phpQsHN3ZAM.jpg
phpQsHN3ZAM.jpg (50.41 KiB) Viewed 252798 times
Still playing with silver foils and alchemy and French vanilla ! oh so fun. I might slump shallow this time for broader affect. Good to have a show with all shapes and sizes . My goal is 12 large vessel forms but will even try for 20. Hmm :-k
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Pat K.
Posts: 53
Joined: Thu Aug 04, 2005 12:33 pm
Location: Pittsburgh, PA

Re: New Alchemy / Silver Experiements

Post by Pat K. »

Beautiful as always. You inspire us all, and I thank you for your many posts. I can't imagine the amount of glass that you go through as well as the time and energy that it takes to do each piece.

Patty
Patty

It often shows a command of language to say nothing - author unkown.
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

Let me just say that husbands are not as enthusiastic as I am but oh dear eh!! just must create and experiment and create some more. You know what I am finding out tooo is that different silver foils are reacting incredibly different . Some are pure than others perhaps. Every colour of the rainbow!!! Oh so fun. Les
P.S. and thanks so much for your kind words.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

New Experiments with Silver and Vitrograph Sky! so much fun. Blending will not be easy to finish this so will have to be a very abstract piece.
phpv3eZQzPM.jpg
phpRu38INPM.jpg
phpNba3JUAM.jpg
Hopefully the Fly Away into Vitro Sky piece will go with my vitro Bowl
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

php7Z56s6PM.jpg
Now the waiting game begins!!!!
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: New Alchemy / Silver Experiements

Post by twin vision glass »

Oh my ,!  dark brooding sky
Oh my ,! dark brooding sky
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Post Reply