I have a chance to buy an  Evenheat GT 14-6 that someone is selling as a glass kiln with Rampmaster 2.
However, when I look at Evenheat's website, they describe the Rampmaster 2 for use in ceramic firing.   Should I buy this kiln if I want to use it for glass?
Debbie
			
			
									
						
							Evenheat with Rampmaster 2.. should I buy it?
Moderator: Tony Smith
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
Re: Evenheat with Rampmaster 2.. should I buy it?
The 14-6 is indeed a glass kiln and should be great for a beginner. The Rampmaster 2 is Evenheat's controller for both glass and ceramic kilns.
Tony
			
			
									
						
							Tony