This seems to the year when all of my tried and true glues are either running empty or have expired.  I have been using the same bottle of White Rain Extra Hold Unscented pump hairspray for years, but when I went to the dollar store to buy another bottle, the new version has "active botanicals".  I am glad to report the botanicals burned away clean, and I am glad I purchased two bottles this time.
Also, my long-time UV glue supplier, Peter Dewey, who represented Dymax, retired a couple of years ago and the last of the UV glue I purchased from him also is just about gone. It has been somewhat of a challenge to find another supplier, even though the representatives were very nice and knowledgeable, because I am such a small purchaser. I am still experimenting, but I was directed to the following website by one of the representatives. The owner of the business is very knowledgeable and is willing to work with craftspeople and sell small quantities.
http://www.clk-llc.com/Adhesive-Selector-Page.html
Sometimes the website is a little slow to load, so have patience.
Tangent was recommended to me by Tom Fuhrman for UV glue, but I was too small to make a minimum purchase. However, Tangent did recommend the above website, and I appreciate Tom's assistance.
Unlike White Rain, UV glues have a one to two year shelf life, so I do need a reliable supplier.
			
			
									
						
							Also, my long-time UV glue supplier, Peter Dewey, who represented Dymax, retired a couple of years ago and the last of the UV glue I purchased from him also is just about gone. It has been somewhat of a challenge to find another supplier, even though the representatives were very nice and knowledgeable, because I am such a small purchaser. I am still experimenting, but I was directed to the following website by one of the representatives. The owner of the business is very knowledgeable and is willing to work with craftspeople and sell small quantities.
http://www.clk-llc.com/Adhesive-Selector-Page.html
Sometimes the website is a little slow to load, so have patience.
Tangent was recommended to me by Tom Fuhrman for UV glue, but I was too small to make a minimum purchase. However, Tangent did recommend the above website, and I appreciate Tom's assistance.
Unlike White Rain, UV glues have a one to two year shelf life, so I do need a reliable supplier.
Lynn Perry
			
						- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Glues - Update
Chuck Karnolt sells UV glues to glass artists and is a very helpful guy.  He has some new fangled LED curing lights.  
http://www.clk-llc.com/
			
			
									
						
							http://www.clk-llc.com/
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
- 
				Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Glues - Update
The best UV glue is Nano470 Construction Glass Glue for heavy and load bearing applications.
You can buy it here:
http://www.dullesglassandmirror.com/sto ... sglue.aspx
Here is it's Australian site with demonstration and instructional videos:
http://www.nano470.com.au/high-strength ... index.html
Pete
			
			
									
						
							You can buy it here:
http://www.dullesglassandmirror.com/sto ... sglue.aspx
Here is it's Australian site with demonstration and instructional videos:
http://www.nano470.com.au/high-strength ... index.html
Pete
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
			
						http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
- 
				Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Glues - Update
Checking the msds that nano stuff does not work with textured or coloured glass.
			
			
									
						
										
						Re: Glues - Update
Bullseye's Mailout this morning promotes a new video on using French cleats. The adhesive they recommend is Dow Corning 995 Silicone Structural Sealant (8617). I haven't watched the video so am not aware of weight restrictions. It may not be transparent either as it's for attaching cleats.......just passing on the reference. Jen
			
			
									
						
										
						- 
				Alexis Dinno
- Posts: 57
- Joined: Sun Dec 13, 2009 9:35 pm
Re: Glues - Update
Hi All,
I have a new project coming up emphasizing lamination of plate glass. I have had quite satisfactory experiences with Loctite 349 and direct sunlight as my UV source. I saw the Nano470 recommendation, and wonder:
1. What are your current favorite clear UV curing glass glues with bond strengths that are comparable to the strength of the glass itself?
2. What are your current recommendations for hand-held artificial UV sources for curing? (I followed Bert's link, but the seems to be some link rot on the product site). Are portable UV-C water/hand sanitizing lamps appropriate?
Best,
Alexis
			
			
									
						
										
						I have a new project coming up emphasizing lamination of plate glass. I have had quite satisfactory experiences with Loctite 349 and direct sunlight as my UV source. I saw the Nano470 recommendation, and wonder:
1. What are your current favorite clear UV curing glass glues with bond strengths that are comparable to the strength of the glass itself?
2. What are your current recommendations for hand-held artificial UV sources for curing? (I followed Bert's link, but the seems to be some link rot on the product site). Are portable UV-C water/hand sanitizing lamps appropriate?
Best,
Alexis
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Glues - Update
Alexis, call Chuck Karnolt.  He knows a lot about gluing glass.
			
			
									
						
							Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: Glues - Update
Cr LAurence sells many different types of UV glues, and have a larger variety than the CLK website. They also appear to be cheaper than the mentioned websites. I buy large amounts from CR Laurence and have great success.
			
			
									
						