100% bullseye glass. 30 inch by 15 inch, 1/2 inch thick. Sandblasted except for the fringe which I treated with etching cream to remove the shine.
image.jpg
glass rug closeup.jpg
glass rug closeup.jpg (39.54 KiB) Viewed 33640 times
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Glass rug

Post by Buttercup »

Delicious!! Jen
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Glass rug

Post by Vonon »

So beautiful! The loose look on the fringe is so realistic and an excellent idea to do the etching on it.
Vonon
Cate G
Posts: 65
Joined: Thu May 05, 2005 6:30 am
Location: Paramus, NJ and Parksville, NY
Contact:

Re: Glass rug

Post by Cate G »

Love the colors. That must have been a tremendous amount of work. Love it!!
Cate
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Glass rug

Post by Sharol »

Wow! This is amazing and with Shawn's typical attention to detail. :wink: . The fringe is wonderful! Beautiful work, Shawn.

Sharol
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Glass rug

Post by JestersBaubles »

Beautiful! Thank you for posting a picture.

Dana W
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Glass rug

Post by twin vision glass »

=D> =D> =D>
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Pat Donaldson
Posts: 25
Joined: Fri Aug 10, 2007 9:45 am

Re: Glass rug

Post by Pat Donaldson »

I can only think of one comment.......COOL!
Judith Andre
Posts: 28
Joined: Thu Mar 20, 2003 2:38 am
Location: Lincoln, NE

Re: Glass rug

Post by Judith Andre »

Nice! I always thought I would do a fused run, but never tried it. Mine would probably not be as beautiful or detailed as this.
Judith
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Glass rug

Post by Havi »

just beautiful!


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Post Reply