alarm warning on jen ken
Moderators: Brad Walker, Tony Smith
-
Nicole Hanna
- Posts: 27
- Joined: Wed Jul 27, 2005 10:17 am
- Location: SW Missouri
- Contact:
alarm warning on jen ken
I'm at a friend's studio and need a quick answer ...she has a jen ken that keeps throwing an "FtC"...failure to cool alarm when it hits about 540 degrees on the way down. Any idea why it's doing this?
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: alarm warning on jen ken
Most likely she has programmed a cooling rate that's faster than the kiln can cool. (FtC = Failure to Cool)
Unless the piece is really thick, she should just turn the kiln off (i.e., end the program) once the temperature gets down to 750 and let it cool naturally.
Unless the piece is really thick, she should just turn the kiln off (i.e., end the program) once the temperature gets down to 750 and let it cool naturally.
-
Nicole Hanna
- Posts: 27
- Joined: Wed Jul 27, 2005 10:17 am
- Location: SW Missouri
- Contact:
Re: alarm warning on jen ken
Thanks Brad. That's what I thought but didn't want to give her bad info if I was wrong.